Brich Plywood With Phenolic Glue Boling Time 72 Hours
video
Brich Plywood With Phenolic Glue Boling Time 72 Hours

Brich Plywood With Phenolic Glue Boling Time 72 Hours

Brown film, Black film, Red film, green PP plasctic,Anti-slip film, with logo,Poplar, hardwood, combi, finger-joint core,birch core,WBP glue,Phenlic glue, For more details pls contact 008618953984274(WhatsApp/Wechat).
Send Inquiry
Product Details ofBrich Plywood With Phenolic Glue Boling Time 72 Hours

For more details pls contact 008618953984274(WhatsApp/Wechat).


Item
Film faced plywood, Construction plywood, Form-work plywood
Film
Brown film, Black film, Red film, green PP plasctic,Anti-slip film,
with logo
Core
Poplar, hardwood, combi, finger-joint core
Hot press
1 time or 2 times
Glue
melamine WBP, phenolic WBP
Size
1220×2440mm,1250×2500mm or as requirement
Thickness
9mm, 12mm,15mm, 16.5mm, 17mm, 17.5mm, 18mm
Thickness tolerance
+/- 0.5mm
Density
500-600 KGS/CBM
Moisture
To be 6%-14% at time of shipment
Usage
Construction, form-work


Hot Tags: brich plywood with phenolic glue boling time 72 hours, China, manufacturers, factory, customized, wholesale, quotation, low price, free sample, made in China, Linyi 18mm Finger Joint Marine Plywood, Fenolico Triplay Double Film For Construction, Birch Core Phenolic WBP Glue Plywood, 4 x8 Water Proof Black Film Faced Plywood, Two Times Hot Press Film Faced Plywood, Finger Joint Core Film Faced Plywood